Adam Dickson

Reflow of fuel inlet strainer

The original soldering was poor - the joint looked cold, and the wetting of the copper tube and brass grille was minimal. The grille was removed and cleaned. The copper tube was cleaned of solder and polished. Acid flux (Baker's) was used with 60%/40% lead tin solder to re-establish a good join to the brass and the copper tubing. The tube was closely inspected for any blockages.